Home/Insights/Selection guide
Selection guide

Antifouling: select by activity profile, not by price

Updated 3 Nov 2026

Three antifouling families solve three different problems. What separates them is how the ship is actually operated, not the price per litre.

Two ships of the same size and, on paper, the same trade can need completely different antifouling systems. One spends most of the year under way at service speed; the other waits at anchor for weeks between voyages. Put the same coating on both and one of them will fail — not because the product was wrong, but because the assumption behind it was.

Three families, three mechanisms

  • Foul release (silicone or fluoropolymer). A low-surface-energy surface that fouling cannot grip. It does not release biocide to do the work; it relies on hydrodynamic shear to shed what has settled, and it gives very low friction while it is clean.
  • Silyl-acrylate self-polishing (SPC). The binder hydrolyses at a controlled rate in seawater and the surface renews itself as the ship moves. Polishing is predictable over long service intervals.
  • Conventional soluble-matrix. A soluble binder with biocide: economical and forgiving to apply, but it leaches quickly when the ship is idle and polishes unevenly at speed.

Measure the profile before choosing

  • Days under way against days idle, at anchor or in port — the strongest single predictor of how a system will behave.
  • Service speed and typical load condition: polishing is driven by shear at the surface, not by calendar time.
  • Water temperature and salinity on the actual route, including any fresh or brackish legs.
  • Planned docking interval, and what the yard can apply and inspect in the time available.
  • Any trade that puts the hull in contact with abrasion: ice, dredging, heavy silt.

Idle time is the dividing line

Foul release depends on movement. A hull that sits at anchor accumulates a settled layer that low surface energy alone will not remove, and the first weeks back in service are spent burning fuel to shed it. Self-polishing systems are more forgiving because the surface keeps renewing, but they slow down when the ship does. Soluble-matrix coatings fail in the opposite direction: an idle hull drains the biocide out of the film before the coating is ever asked to perform. The honest question is therefore not which technology is most advanced, but how many days a year this hull is actually moving — and who is prepared to clean it when it is not.

Where changing family goes wrong

Most antifouling failures do not originate in the topcoat. They originate in the interface beneath it. Moving from a conventional system to a silicone foul release means removing or fully sealing the old coating, because silicone will not bond to a leached self-polishing surface, and a residual soluble layer will delaminate under the new film. A tie coat is not an optional extra. Intercept 8500 LPP, SeaQuantum X200 and Intersmooth 7465HS SPC belong to three different families, and the primer and tie coat beneath each are not interchangeable. The same logic applies to the anticorrosive scheme: an epoxy such as Intergard 263 is a sound base for any of them, but only on steel prepared to the specified standard and overcoated inside the specified window.

What the specification has to state

  • Total dry film thickness and the number of coats, given per coat rather than as a single total.
  • Tie coat type and its own thickness, and whether it counts towards the total.
  • Minimum drying and immersion time before the ship leaves the dock. A system applied and floated the same day is a system that has not finished forming.
  • Inspection: thickness per coat, holiday detection where specified, and a signed record of batch numbers, application conditions and measured steel temperature.

None of this replaces the manufacturer's documentation. Specific parameters follow the latest technical data sheet (TDS) for the product concerned; publicly available manufacturer materials explain the mechanism, not the warranty.

The rule in one line

Choose the family that matches how the ship moves, then choose the product inside that family on docking interval and yard capability. Price then becomes a comparison between like systems, which is the only comparison that means anything. A cheap conventional coating that has to be cleaned twice a year is not cheaper than a foul release system that does not — and a premium system applied over the wrong tie coat is not premium at all.

Sources

  • International Convention on the Control of Harmful Anti-fouling Systems on Ships (AFS Convention, 2001, as amended), public scope
  • IMO 2023 Guidelines for the control and management of ships' biofouling to minimize the transfer of invasive aquatic species (resolution MEPC.378(80)), public scope
  • ISO 12944-5, Protective paint systems for steel structures — protective paint systems, public scope
  • Publicly available manufacturer materials and product data sheets for the antifouling systems named in the text; specific parameters follow the latest technical data sheet (TDS) of the product concerned

Articles are compiled by RichTech from publicly available manufacturer materials and field practice, for selection reference only; the latest official technical data sheets (TDS) prevail.

Not sure which product fits? Tell us the substrate and service conditions

Share your substrate, corrosivity category and target service life — we will come back with a coating system and quantity estimate.